Reverse Osmosis
Sea Water
HS-Thin Film Composite Sea Water
Element Specifications
Model |
Flow Rate
GPD
(M3/D) |
Average
Rejection
(%) |
Surface
Area
(ft2) |
Dimension
(in) |
| A |
B |
C |
HS-SW2-2540FF* |
3,80(1.47) |
99.6 |
25 |
40 |
2.38 |
0.750 |
HS-SW2-4040FF* |
1,300(4.92) |
99.6 |
80 |
40 |
3.88 |
0.750 |
HS-SW2-4040F |
1,400(5.30) |
99.6 |
85 |
40 |
3.88 |
0.750 |
HS-SW2-8040F |
6,000(22.73) |
99.6 |
370 |
40 |
7.88 |
1.125 |
Performance is based on 32,000 ppm NaCl solution at 800
psig operating pressure, 77°F(25 °C) and 7% recovery. Individual element performance may
vary up to 15%.

Operating Parameters:
| Temperature: |
Maximum 50
°C |
| pH: |
2-11 (CIP:
1-11.5) |
| Pressure: |
Maximum
1,200 psig |
| Free
chlorine: |
Maximum
<0.l ppm |
| Silt
density index: |
Maximum 5 |
| Differential
pressure: |
Maximum 15
psig per element not to exceed 60 psig per housing. |
*Stinger design
Rejection Characteristics
Ions |
HS-SW1 Elements |
HS-SW2 Elements |
Sodium, Na+ |
99.5 |
99.6 |
Potassium, K+ |
99.4 |
99.4 |
Calcium, Ca+2 |
99.6 |
99.7 |
Magnesium, Mg+2 |
99.3 |
99.8 |
Chloride, Cl- |
99.6 |
99.5 |
Alkalinity, HCO3- |
98.9 |
99.5 |
Sulfate, SO4-2 |
99.7 |
99.8 |
Nitrate, NO3- |
99.5 |
99.2 |
Silica, SiO2 |
98.9 |
98.8 |
TDS |
99.6 |
99.7 |
Performance is based on
32,000 ppm sea water at 800 psig operating
pressure, 77°F (25 °C) , pH 8.1 and 7% recovery. Individual element performance may vary